http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07330851-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-685 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-32 |
filingDate | 1994-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_baf7ffadd02c2ecc2f84bade6bd97618 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8811dc7b954dd3319f54a5f1527cb4b4 |
publicationDate | 1995-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07330851-A |
titleOfInvention | Thermoplastic polyurethane and thermoplastic polyester |
abstract | (57) [Summary] [Purpose] To provide a thermoplastic polyurethane having excellent heat resistance and durability and good mechanical properties. [Structure] A thermoplastic polyurethane containing a diamino compound represented by the following general formula (I) and a diisocyanate as a main component, wherein a die having a diameter of 1 mm and a length of 10 mm is used in accordance with JIS K 7210 and a load of 100 kg. Melt viscosity measured at f / cm 2 is 5 × 10 at 185 ° C. 3 poise or more, 1 × 10 6 poi at 225 ° C. A thermoplastic polyurethane characterized by being less than or equal to se. In the formula, R 1 and R 2 independently represent a residue obtained by removing an amino group from a diamino compound having a molecular weight of 46 to 500. |
priorityDate | 1994-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 250.