http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07323261-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 |
filingDate | 1994-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51a37994ec1bf58042dfc1ff2ac43e6d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f13111d35b1e3e75e6cb012da3836c4d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e9d18dba5b5abb5c5372973e4a7b863 |
publicationDate | 1995-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07323261-A |
titleOfInvention | Method for manufacturing coating film |
abstract | (57) [Summary] [Structure] A coating composition comprising a silane compound (A) having an amino group and a compound (B) having a functional group capable of reacting with the amino group in the silane compound is applied to a substrate. After that, it is dried in a warm / humidified atmosphere to form a film, And / or after forming a dry film of the coating composition, aging treatment is performed in an atmosphere of 20 to 60 ° C. and 5 to 80% RH. [Effect] Excellent water resistance, chemical resistance, weather resistance, and heat resistance, In addition, a coating film excellent in flexibility, particularly a gas barrier film, can be produced with good productivity without impairing these physical properties and without causing tacking. Even if the amount of water in the coating composition is reduced, the film is formed in a heated / humidified atmosphere or is subjected to aging treatment in a heated / humidified atmosphere, so a stable, high-performance gas barrier film. Can be obtained. In addition, the storage stability of the coating composition could be significantly improved. |
priorityDate | 1994-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |