http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07315941-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B37-00 |
filingDate | 1994-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3bfb55fffb7c6911cafc7d801b76b66b |
publicationDate | 1995-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07315941-A |
titleOfInvention | Binder composition |
abstract | (57) [Summary] [Object] To provide a binder composition for forming a ceramic, which has a dense structure and can obtain a green sheet that can be made into a thin film. A binder composition comprising 3-methyl-3-methoxy-1-butanol and at least one binder selected from polyvinyl acetate, partially saponified polyvinyl acetate and polyvinyl acetal. [Effect] It is possible to make the film thinner than before in the production of green sheets, and various high-performance ceramic electronic components can be obtained from these green sheets. Further, since it has a large adhesive force, it is useful not only for forming ceramics but also as an adhesive for laminated glass, for example. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101586014-B1 |
priorityDate | 1994-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 44.