http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07315928-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1476752f2420c8f8eb53464cf7fc922b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-495 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-00 |
filingDate | 1994-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24aa5648b6cb6627609908da58b97692 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8597ba00fa1f8505bb10b10abfd66b0a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6a46f57d5a3d9bd2c8d41cdad15ba8e |
publicationDate | 1995-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07315928-A |
titleOfInvention | Method for producing lead-containing ceramic powder |
abstract | (57) [Summary] [Object] To provide a method for producing a lead-containing ceramic powder excellent in low-temperature sinterability in which a trace amount of additives such as a sintering aid is uniformly dispersed. [Structure] General formula PbMO 3 (where M is 1 or more of 2 In the production of a lead-containing ceramic powder represented by a hexavalent metal element), a powder having a composition of PbMO 3 is dispersed in a solvent to form a slurry, and the metal salt compound is dissolved in the slurry to prepare the powder. After mixing with the body, after drying the slurry to support and fix the metal salt compound on the powder surface, This powder is characterized by being calcined. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007191351-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004168637-A |
priorityDate | 1994-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.