http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07310134-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9f8d2c54eb3f61af08e82568018c8e3b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-055 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C21-00 |
filingDate | 1994-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a031ebb54eba310794d6a1f36d6854cb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_843b6ff3f256e2e2a24827c924d77933 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b2ffde644a920d7c97f2f3769088966f |
publicationDate | 1995-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07310134-A |
titleOfInvention | Aluminum foil for electrolytic capacitor anodes and aluminum foil for electrolytic capacitor anodes |
abstract | (57) [Summary] [Purpose] The main purpose of the present invention is to provide an aluminum foil for an electrolytic capacitor anode and a material thereof that exhibit high bending strength even after heat treatment and chemical conversion treatment. [Configuration] 1. An aluminum foil base material for an electrolytic capacitor anode, wherein the purity of aluminum is 99.9% or more and the content of sodium is 0.01 ppm or less. 2. An aluminum foil for an electrolytic capacitor anode, wherein the purity of aluminum is 99.9% or more and the content of sodium is 0.01 ppm or less. |
priorityDate | 1994-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |