http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07292357-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5073c72837c69a4850d017e75290dd1
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00732
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0039
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K103-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K17-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E02D3-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K17-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K17-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K17-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02
filingDate 1994-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e9da64d1b7156e7399bf6b4866e8c966
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2277515c8c7d5f28fd05336d43414652
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f8fa4caa250951f543b3acad46f93508
publicationDate 1995-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-H07292357-A
titleOfInvention Soil stabilization chemicals and ground stabilization method using the same
abstract (57) [Summary] [Structure] In a soil stabilization chemical solution combining a liquid A containing Portland cement and a liquid B containing alumina cement, a liquid A is a cement expansive material, and a liquid B is an inorganic carbonate. Each of the salts is mixed, and in the mixed solution of the liquid A and the liquid B, the cement expansive material is 15 parts by weight or more per 100 parts by weight of alumina cement, and the alumina cement is 18 parts by weight per 100 parts by weight of Portland cement. It is mixed and used so that the amount of the inorganic carbonate is 2 to 9 parts by weight. [Effect] Even if the solution A and the solution B are left without adding a setting retarder, they are not cured in less than 3 hours after the preparation and have high stability, while the solution mixture of the solution A and the solution B has a high stability. It cures within minutes, and the formed cured product exhibits good compressive strength, and has stability, quick-setting property, and early-strength property.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9102870-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009209293-A
priorityDate 1994-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451818717
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID453688467
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID31357
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559505
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3084047
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419524917
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID157010056
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID452450317
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID9989226
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5460341

Total number of triples: 34.