http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07278302-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_47cc435e1d443f13180f7766df104d9d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-685 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-08 |
filingDate | 1994-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f9ca255b7d5d077fa20d190e621c2d1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a117b0916be73e19e8d2e92336f8583 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a5684c61a4af9fd6111997a81d0c2d62 |
publicationDate | 1995-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07278302-A |
titleOfInvention | Process for producing polyesterimide, heat-resistant resin composition and insulated wire |
abstract | (57) [Abstract] [Purpose] A method for producing a polyesterimide having a solderability, an excellent heat resistance, and a high softening temperature, and a heat-resistant resin composition using the same. And provide insulated wires. [Structure] 5 to 50 equivalent% of cyclo ring-containing glycol and 5 to 5 of tris-2-hydroxyethyl isocyanurate Method for producing polyesterimide by heating reaction of alcohol component containing 30 equivalent% and acid component containing 10 to 70 equivalent% of imide group-containing polycarboxylic acid, heat-resistant resin composition containing the polyesterimide, and composition thereof Insulated wire that is made by applying and baking objects on a conductor. |