http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07257954-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04 |
filingDate | 1994-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fa5e9ba76e8eaab7299110c6cc7bd6d8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ae8efd9de63f69504a9670d76f88bba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50458c5ed8166266a62fcb40a369263c |
publicationDate | 1995-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07257954-A |
titleOfInvention | Hardened cement |
abstract | (57) [Summary] [Purpose] To provide a hardened cement product mainly used in the civil engineering and construction industry. [Constitution] 100 parts by weight of cement having a 3CaO / SiO 2 content of 60% by weight or more, 1 to 5 parts by weight of anhydrous gypsum, 0.2 to 3 parts by weight of aluminum sulfate in terms of anhydride, and an alkali metal aluminate salt. A hardened cement product is obtained by mixing a cement composition containing 0.1 to 0.8 parts by weight with water. [Effect] The hardened cement product according to the present invention has effects such as good initial strength development even without steam curing. |