Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6ee5332511e21d1f63564d84b98214c9 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 |
filingDate |
1994-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_291e305b44cbeee75a54e18df25fa37f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b536d149582a24387969c7faf3df9e02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_023085158df8d76976f96ae61a280369 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_27268e8d8e23e2885443d684f127706a |
publicationDate |
1995-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H07228722-A |
titleOfInvention |
Method for obtaining recycled resin composition |
abstract |
(57) [Summary] [Objective] To provide a method for reclaiming a coated molded article by a simple method without polluting the environment to obtain a reclaimed resin composition having excellent initial mechanical properties. To do. A method for obtaining a recycled resin composition from a molded article having a coating film, which comprises a resin composition containing a polyphenylene ether (PPE) resin and a polyamide (PA) resin. (A) 10 to 80 parts by weight of PPE resin and (B) 90 to 20 parts by weight of PA resin having an amount of terminal amino groups of 0.05 meq / g or more, and the total of (A) and (B) A regeneration auxiliary material composition containing 25 to 75 parts by weight of the (C) rubber-like polymer is mixed with 100 parts by weight of the crushed product of the molded article having the coating film, and the mixture is melt-kneaded. The regeneration auxiliary material composition and the regenerated resin composition obtained by the method. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002105332-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003014190-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002338827-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0053384-A1 |
priorityDate |
1994-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |