Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6cfc033f059d282fcd915bc8be2ae53f |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 |
filingDate |
1994-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f652c96e2861b8365f72c29d5241de3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a371c866fa962e2924d6331443e639f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_220b63f7b414203c25bfedecb7130531 |
publicationDate |
1995-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H07216126-A |
titleOfInvention |
Low foaming fiber reinforced resin composition and molded product thereof |
abstract |
(57) [Summary] [Structure] A resin composition comprising a thermoplastic resin and 5 to 100 parts by weight of a fibrous reinforcing material with respect to 100 parts by weight of the resin, and containing an effective amount of a foaming agent. Low foaming fiber reinforced resin composition and molded products thereof. [Effects] Molded products obtained by melt-molding the composition of the present invention have excellent mechanical properties, warp deformability of the molded products, The dimensional stability is remarkably improved and it can be used for many purposes. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003253118-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005305744-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09255872-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5843568-A |
priorityDate |
1994-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |