http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0718224-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_250d7d24d096f307230e703f0ddc2275 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 |
filingDate | 1993-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02646fc44a50834bf042173678f48e7c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3c9fbebfcb8271ba92a3f39982bc0ef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4341adcdf99390b9f80dcbd7f102c5a0 |
publicationDate | 1995-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0718224-A |
titleOfInvention | Wire binding tape |
abstract | (57) [Summary] [Purpose] To provide a wire binding tape having a high degree of flame retardance and no generation of toxic gas even when burned, and having safety, flexibility, mechanical characteristics, and electrical insulation. To do. [Structure] The base material of the electric wire binding tape is a polyolefin resin composition. The polyolefin resin composition, An inorganic flame retardant is blended in an amount of 8 to 28 parts by weight based on 100 parts by weight of the polyolefin resin. Further, 8 to 24 parts by weight of the inorganic flame retardant of 8 to 28 parts by weight is red phosphorus. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7818941-B2 |
priorityDate | 1993-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 35.