http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07164140-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_40c1bcb35511762bd1a6c2dd10d52a17 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K1-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K1-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-34 |
filingDate | 1993-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e134a9fb58832c6bfdd8a2ad24ef662 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2da19c4f6a5424ea7a84730667e5b69a |
publicationDate | 1995-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07164140-A |
titleOfInvention | Method of manufacturing aluminum material for brazing, and brazing method |
abstract | (57) [Summary] [Purpose] Avoids the problems of ordinary non-corrosive fluoride flux brazing, which is caused by applying flux after assembling into a complicated product shape, and also using Mg as a getter material. Vacuum brazing is possible without using a large amount as in the past. [Constitution] The aluminum material contains one or two of borofluoric acid and hydrosilicofluoric acid in a total amount of 0.01% to 40%, or one or two of nitric acid, sulfuric acid, phosphoric acid and chromic acid. An aqueous solution containing at least one species at a temperature of 5 ° C to 70 ° C for 1 second to 2 Process for 0 minutes. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007069266-A |
priorityDate | 1993-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |