http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07148241-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-16 |
filingDate | 1994-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11ebd600d2f0bda408585b42b60296e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1342c84ddf2c014fafd6863339446d5d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46eb576ce8fd97bf70d2585b0753bc93 |
publicationDate | 1995-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07148241-A |
titleOfInvention | First aid bandage film |
abstract | (57) [Summary] [Purpose] It is made of non-PVC resin, contains virtually no plasticizer, has flexibility and stretchability, and has fast stress relaxation during stretching, does not press the affected area and has a texture. Providing a good film for first aid bandages. [Structure] A film for an emergency adhesive bandage in which at least a polypropylene resin layer and an olefinic thermoplastic elastomer layer or a styrene thermoplastic elastomer layer are laminated. Further, at least the polypropylene resin layer, and the olefin thermoplastic elastomer layer and the styrene thermoplastic elastomer layer may be laminated. The polypropylene resin has a weight average molecular weight of 8 The composition is in the range of 50,000 to 500,000, and has a predetermined resin elution amount in the predetermined temperature range by the cross fractionation method. |