http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07146592-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-113 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-107 |
filingDate | 1994-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86b8458adb107b802b24c6c26b8d7482 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_55876dec336cdd8f7794468c696f14b6 |
publicationDate | 1995-06-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07146592-A |
titleOfInvention | Two-component developer for electrostatic latent image development |
abstract | (57) [Summary] [Object] To provide a dry two-component developer that suppresses temperature dependence, effectively prevents the spent of toner on the surface of a carrier, and obtains an image having no edge effect. [Structure] Magnetite having a concentration of an alkali metal salt present on the surface of 0.15 μg / cm 2 or less is used as carrier core particles. The surface of the carrier core particles here is coated with a resin to form the original carrier particles. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6025103-A |
priorityDate | 1993-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 83.