http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07133399-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_52a65b677bbedbe7bf090dd556a7cc43 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 |
filingDate | 1993-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_053744ee086f6ae8cde206c599b5b84e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dfddf80ca0b059d2b442646c8ddc0de9 |
publicationDate | 1995-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07133399-A |
titleOfInvention | Crystalline propylene polymer composition |
abstract | (57) [Summary] [Object] To provide a crystalline propylene polymer composition which is excellent in tensile elongation, impact resistance and thermal rigidity of a molded product. [Structure] Isotactic pentad fraction (P) and melt flow rate (MFR) of crystalline propylene homopolymer The first stage polymer having a relationship with 1.00 ≧ P ≧ 0.015 log MFR + 0.955 is 70 to 95% by weight of the total amount of polymer, and then 30 to 5% by weight of the total amount of ethylene or ethylene and propylene. To 100 parts by weight of a crystalline ethylene-propylene block copolymer having an ethylene content of from 3 to 20% by weight based on the total amount of the polymer obtained by polymerizing at least one stage. Alternatively, a crystalline propylene polymer composition containing 0.001 to 1 part by weight of an amino acid diamide. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0854155-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0854155-A1 |
priorityDate | 1993-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 468.