http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07118973-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-04 |
filingDate | 1993-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aade90740629471af33a5f5e44b5ca59 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b3c9054c7942c055768199407c44d87 |
publicationDate | 1995-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07118973-A |
titleOfInvention | Method for producing deep-dyeing special mixed yarn |
abstract | (57) [Summary] [Purpose] It has no stain spots and is excellent in bathochromic properties. Provided is a method for producing a deep-dyeing special mixed fiber that can be used as a fabric having a soft texture with tension and elasticity. [Structure] A plurality of polyester undrawn yarns having a breaking elongation difference of 300% or more and a birefringence difference of 0.06 or more are aligned and subjected to an entanglement treatment, and then a processing magnification of 1.10 to 1.4. At 0, heating is performed so that the yarn temperature immediately after the heater exit is 70 to 100 ° C., a false false twisting process is performed, and then 150 Heat treatment at ℃ or above. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100546463-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115012089-A |
priorityDate | 1993-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |