http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07118354-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1d29f7ac2c7f9be9f7dae1a83bbb5c92 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F297-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-60 |
filingDate | 1993-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e60b3516ff5fe792135a27a3e63a3cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c7517fe04d118e639399933fbceb783 |
publicationDate | 1995-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07118354-A |
titleOfInvention | Propylene ethylene block copolymer composition |
abstract | (57) [Summary] [Purpose] To obtain a propylene ethylene block copolymer composition excellent in transparency, tensile elongation, gloss and tensile elongation. [Composition] Melt flow rate is 0.01 to 100 g / 1 It is 0 min, the ethylene content is 10 to 50 mol%, and the elution curve is represented by the temperature (° C.) on the horizontal axis and the integrated weight ratio (wt%) on the vertical axis. In this case, the elution component (A component) below 30 ° C is 20 ~ 80 wt%, elution component (B The component) is 15 to 75 wt%, the elution component (C component) at 70 ° C. or higher is 5 to 70 wt%, and the elution amount of B component in the elution curve divided at every 10 ° C. is at least 3 wt%. A propylene ethylene block copolymer composition. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006008782-A |
priorityDate | 1993-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 112.