http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H07102078-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 1993-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_33b79f6d5f343051bae00fd9b89ba089 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3458e782bd7cf18dac5353202dfe5759 |
publicationDate | 1995-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H07102078-A |
titleOfInvention | Water absorbent material and method for producing the same |
abstract | (57) [Summary] [Purpose] A water-absorbing material which is supple and has good water absorption (water absorption rate and water absorption amount), can be cut into any size or shape, and is highly safe, and the water-absorbing material. To provide a simple and highly productive production method for controlling the product performance. [Structure] (a) a step of obtaining a mixture of water-absorbent resin particles and a polyhydric alcohol; (b) the mixture obtained in step (a) and a hydrophilic fiber are mixed with water-absorbent resin particles 100 in the mixture. Production of a water-absorbing material comprising a step of dry-mixing hydrophilic fibers at a ratio of 1 to 30 parts by weight with respect to parts by weight, and (c) a step of air-paper-making the mixture obtained in step (b) into a sheet form. Is the way. |
priorityDate | 1993-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |