Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06C7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C71-02 |
filingDate |
1992-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_40ad236531f6a588c1344bc1011857cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47e661bd7418ad2e32bf3d6762c9cf4c |
publicationDate |
1994-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0699511-A |
titleOfInvention |
Method for producing polyester fiber or molded product |
abstract |
(57) [Summary] [Structure] A fiber or molded article is formed from a polyester composition in which a phosphite type antioxidant is mixed in a copolyester having a polyoxyalkylene chain in the molecule, and the temperature is 100 ° C or higher. A method for producing a polyester fiber or a molded product, which is heat-treated at a temperature of 3 hours or more. [Effect] A modified polyester fiber or molded article having no discoloration such as yellowing can be obtained. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021070897-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106414549-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015186653-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011117092-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016191177-A |
priorityDate |
1992-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |