http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H069830-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_68496d12a251010a470395787518f996 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 |
filingDate | 1992-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_48a3aa99fe80c5cb65c1b8a5c04250f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_689d30f69e0e0e93b3ee7562567b2c22 |
publicationDate | 1994-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H069830-A |
titleOfInvention | Method for producing polyethylene resin for monofilament |
abstract | (57) [Summary] [Object] To provide a method for producing a polyethylene resin for a monofilament, which has a high maximum draw ratio when formed into a monofilament, is excellent in high-speed stretch moldability, and is less likely to cause rough skin. [Structure] 1 × 10 5 to 4 × 10 5 weight average molecular weight, 1 × High-density polyethylene having a number average molecular weight of 10 4 to 8 × 10 4 and a weight average molecular weight / number average molecular weight ratio of 4 to 10 0.001 to 0.02 parts by weight of a peroxide is mixed with 0 parts by weight, and this is melt-kneaded to form a slightly crosslinked structure. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012510570-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101025038-B1 |
priorityDate | 1992-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.