http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0673246-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 |
filingDate | 1992-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c141192d8e5d351ddb9e832e36d6778 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae3d45bbac5b80013dee053dae0a69bf |
publicationDate | 1994-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0673246-A |
titleOfInvention | Composition for molding sheet material |
abstract | (57) [Summary] [Object] To provide a composition for molding a sheet, which is excellent in flexibility and transparency. [Structure] (a) A block having at least one vinyl aromatic monomer having a number average molecular weight of 2,500 to 40,000 and isoprene or isoprene-butadiene, and the content of 3,4 bonds and 1,2 bonds is 25% or more. The number average molecular weight of the block is 300 Hydrogenated product of block copolymer of 00 to 300,000 90 to 10 parts by weight and (b) 10 to 90 parts by weight of polypropylene are blended to obtain a composition. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002096426-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6833411-B2 |
priorityDate | 1992-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.