http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0664320-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_663cad2cddb9415ae5ba8d9c99803cda |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-26 |
filingDate | 1992-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45341d220a7dfb01665951bd5183e0bf |
publicationDate | 1994-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0664320-A |
titleOfInvention | Thermal recording material |
abstract | (57) [Summary] [Structure] A heat-sensitive recording material having a heat-sensitive recording layer containing, on a support, a colorless or light-colored basic dye and a developer capable of developing a color by reacting with the dye, 4'-isopropylidenediphenol, 4,4'-dihydroxydiphenyl sulfone, bis- (3-allyl-4-hydroxyphenyl) sulfone and bis (4-hydroxyphenyl) At least one developer selected from sulfone and 2 -Benzyloxynaphthalene or p-benzylbiphenyl and at least one kind of sensitizer selected from di (p-methylbenzyl oxalate) and N-methylol fatty acid amide are combined and dispersed in the same mixing system for pulverization. With an esterification degree of 50% or more and an average molecular weight of 1 A heat-sensitive recording material using a styrene-maleic anhydride copolymer ammonium salt of 0000 to 60,000. According to the present invention, it is possible to provide a heat-sensitive recording material having good stability, excellent color development in a low energy region, and good storage characteristics. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017177346-A |
priorityDate | 1992-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 71.