http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0653090-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-00 |
filingDate | 1992-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de331036700da249c2c87e20ec00d205 |
publicationDate | 1994-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0653090-A |
titleOfInvention | Solid electrolytic capacitor and method of manufacturing the same |
abstract | (57) [Summary] [Object] To provide a solid electrolytic capacitor having a large capacity per unit area of an anode substrate and a method for manufacturing the same. [Arrangement] A right-angled triangular anode portion is provided on a part of a rectangular anode substrate 4, and a trapezoidal semiconductor layer 7 and a conductor layer thereon are formed on the remaining portion. |