http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0649507-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2dcebf5a7f7ddc3b081f70e8ce1c4097 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-26 |
filingDate | 1992-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af29e8e2d55814158f4745f1a855d40e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_986c19b2cf80125686fcdef445343e5a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2446ecc35e08e9aed2069d59e77ec0f7 |
publicationDate | 1994-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0649507-A |
titleOfInvention | Method for manufacturing metal powder infiltration molded product |
abstract | (57) [Abstract] [Purpose] To manufacture metal powder infiltration molded products with high accuracy and without requiring post-processing. [Composition] A slurry in which a metal powder for sintering, an organic binder, and water or an organic solvent are mixed is injected into a molding die and pressurized, The liquid component in the slurry is deliquored, powders are brought into contact with each other, and a solidified powder compact is obtained through a binder, and the powder compact is sintered, and then a molten metal is added to the pores of the sintered compact. In the method for producing a metal powder infiltration molded product, the flatness of the sintered body is 0.1 mm or less when the molten metal is infiltrated into the pores of the sintered body. Is placed, and the molten metal is dropped from above the sintered body to impregnate the sintered body. |
priorityDate | 1992-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links