http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0649118-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2f92fe8c03f7c3909756858a67d30a9f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 |
filingDate | 1993-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b780c780a6e50cf56b7d6e9c2635d275 |
publicationDate | 1994-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0649118-A |
titleOfInvention | Method for producing a functionalized resin |
abstract | (57) [Summary] [Object] To provide a simple method for introducing a thiol group into a styrene-divinylbenzene resin. [Structure] Styrene and divinylbenzene in a weight ratio of about 1 to 3 to about 1: 0.1, A process for producing a functional group-containing resin, which comprises suspension-polymerizing a free-radical initiator at a temperature of about 60 ° C. to about 90 ° C., wherein an alkyl at a time of 15% or more and 80% or less of the total polymerization time has elapsed. - di - introducing thiol polymerization mixture, the alkyl - di - thiol C 2 -C 6 alkyl groups and added in an amount of from about 5% to about 20% by weight, based on the sum of styrene + divinylbenzene, and continuing the polymerization to give a thiol-functionalized styrene-divinylbenzene resin. To generate. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008239781-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5393332-A |
priorityDate | 1992-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 93.