http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06329890-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate | 1993-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f14131a328f1eafc04bbc86d5e43f183 |
publicationDate | 1994-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06329890-A |
titleOfInvention | Polyester resin composition |
abstract | (57) [Summary] [Structure] For polyester resin pellets (A), Formula; Tp-20 ≧ Ts ≧ 50 [wherein, Tp = Vicat softening temperature (° C.) of polyester resin, Ts = Vicat softening temperature (° C.) of thermoplastic resin] Vicat softening temperature Based on the weight of the polyester resin pellets (A), the thermoplastic resin pellets (B) having (Ts) of 0.01 to A polyester resin composition containing 10% by weight. [Effect] The polyester resin composition of the present invention has good plasticizing properties, can be plasticized in a short time by a screw type plasticizer, etc., and has a high cooling and solidification rate, so that high productivity and mechanical properties can be achieved in a short time. It is possible to manufacture molded products with excellent physical properties such as strength and thermal properties, and since it does not contain powdery or liquid mold release agents, spreading agents, etc., contamination of molding equipment, molds, incidental equipment, molding There is no clogging in the material supply section of the device, and handling and molding properties are extremely good. |
priorityDate | 1993-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |