http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06325778-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0950e9df7f0e1b73efee1bda859951ad |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 |
filingDate | 1993-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3e63eabc28268569fba5f7cfff7ad32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7883b7e0f2d716b71f9adf843370b4c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b1458692d3050d5aa3a1d3c3ff1bdeed |
publicationDate | 1994-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06325778-A |
titleOfInvention | Molten carbonate fuel cell |
abstract | (57) [Summary] [Object] To provide a molten carbonate fuel cell capable of significantly extending the time until a short circuit occurs inside the cell and thereby maintaining the cell performance for a long term. [Structure] Prevents the primary particles of the oxidizer electrode constituent primary particles, which are composed of carbonate-stable oxides or complex oxides and float / diffuse from the oxidizer electrode 4, from floating / diffusing in the electrolyte layer 1. The trapping layer 3 is provided in the electrolyte layer 1. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003007315-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9853513-A1 |
priorityDate | 1992-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.