Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d7576285d411d00c697e07270d2814a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_abc376cf033a65eda49a51a9cddf4956 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C10-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B19-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C10-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-078 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B32-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-112 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C10-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-097 |
filingDate |
1993-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1ca12ceb027594cf89265fbed4ff1e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ca3ed7751fc4691e1ea95675183da71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dca70330fdd4ad25115bafd422a23917 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8727b9719f2c84a8a99ec05ceb253b0 |
publicationDate |
1994-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H06305827-A |
titleOfInvention |
Manufacturing method of machinable glass ceramics |
abstract |
(57) [Summary] [Purpose] To obtain a glass-ceramic which is less likely to be cracked or chipped and has machinability excellent in properties such as heat resistance, electrical insulation, and mechanical strength. [Constitution] Crystallized glass powder A 25-95% by weight of specific composition And 5 to 75% by weight of crystallized glass powder B are pressure-molded to prepare a plate-shaped body, and the plate-shaped molded body is surrounded by granular or scaly fluorine-containing minerals. Installed in a refractory container at an angle of 15 to 65 ° with respect to the hearth of the firing furnace and heat-treated at a temperature of 1050-1100 ° C. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100348525-C |
priorityDate |
1993-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |