http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06302414-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5736c85c1929ce4e9775e836a65d6c05 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-06 |
filingDate | 1993-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b60cbd4e32c9394058d776ed3b3d969d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fe87108b845c7ce0c1e87c48508f52ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f463a86c5d22a1b0876fbb51b5e2fcf |
publicationDate | 1994-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06302414-A |
titleOfInvention | Method for producing metal magnetic powder for magnetic recording |
abstract | (57) [Summary] [Object] To provide an industrially advantageous method for producing a magnetic metal powder, which is extremely suitable for a magnetic recording medium. [Structure] An iron compound mainly containing iron oxide hydroxide or iron oxide is granulated and molded in the presence of carboxylic acids having 6 or more carbon atoms, and then heat-treated at a temperature of 300 to 800 ° C. in an inert gas atmosphere, Then, it is subjected to heat reduction treatment to obtain a magnetic metal powder for magnetic recording. |