Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5198a2a21392d6cbc0bb4898b3fb3d29 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D11-00 |
filingDate |
1993-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5be5f489745cabfec4332b779abcab24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b92a6598be7f57569bb1da218e0e9e40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de68ea35c63424a7b13b8d831795cfe8 |
publicationDate |
1994-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H06285595-A |
titleOfInvention |
Method for producing multilayer amorphous alloy ribbon |
abstract |
(57) [Summary] [Object] To provide a method for producing a multilayer amorphous alloy ribbon having excellent amorphousness and flatness. [Structure] In the production of a multilayer amorphous alloy ribbon using the multiple slit method, alloys are combined so that the difference in melting point between alloys forming adjacent layers is 80 ° C. or less. [Effect] It is possible to stably obtain a flat amorphous flat ribbon having no warp or edge waviness due to thermal stress generated in the cooling process. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1198605-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1198605-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1452617-A1 |
priorityDate |
1993-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |