http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06277622-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B13-12 |
filingDate | 1993-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_711d6611de657c493845cef9f2ef2cbb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_818edfb3a9b9b31c23d75ea80b34daf0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc42e46388f9b8cf18a5f5c9f5203ce7 |
publicationDate | 1994-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06277622-A |
titleOfInvention | Method for protecting alkaline inorganic cured body and alkaline inorganic cured body having coating film formed by the method |
abstract | (57) [Summary] [Purpose] The alkaline inorganic cured product is extremely resistant to deterioration even when it comes into contact with water, heat, etc., or even under long-term alkaline conditions or high temperature conditions. A method for protecting an alkaline inorganic cured material, which is capable of forming an extremely highly practical protective film excellent in various film properties such as sufficient weather resistance against exposure, It is to provide this cured product having a coating film formed by such a method. [Structure] Applying an aqueous dispersion of fine particle polymers having a multi-layer structure and containing fluoroolefin-based monomers as an essential component as a top coat on an alkaline inorganic cured body; the aqueous dispersion When a coating composition containing a body is applied directly to the cured body or indirectly through a coating layer formed from another coating composition containing such a coating composition, Prior to application of any of the coating compositions of, or after application to form a coating film, the cured product is hydrate-cured under specific temperature conditions in the presence of water. The main configuration requirements are; |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002502449-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015174909-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6262863-A |
priorityDate | 1993-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 138.