Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate |
1992-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a238dfeaa6abc4916747a9850114a8a2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9d2bc354aed469d0389c79090963196 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9be11973fb3ff0ddb27745bcbc081bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4cae5738100d5a472ae7e2aa47fdb9c9 |
publicationDate |
1994-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0627726-A |
titleOfInvention |
Cross-linking resin for image forming toner |
abstract |
(57) [Abstract] [Purpose] To produce a resin for an image-forming toner which is excellent in low-temperature fixability and offset resistance, and has low humidity resistance dependency. [Structure] Compared with a conventional polyester resin, a component from a polystyrene polymer containing an ester bond-forming group having a weight average molecular weight of 50,000 or less is contained in an amount of 50% by weight or less based on the total condensed polyester. The present invention relates to a crosslinked resin for image forming toner having a glass transition point of 40 to 75 ° C. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9923534-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1519242-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0916019-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015105295-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6326115-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03057763-A1 |
priorityDate |
1992-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |