http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06272172-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-144 |
filingDate | 1993-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_37cde37787a50899919bc9a953686218 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98ed5b8ba3478624abc5568464bb2287 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3683d89377aecef92f5e546acd0d9664 |
publicationDate | 1994-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06272172-A |
titleOfInvention | Modified fiber structure and method for producing the same |
abstract | (57) [Summary] [Constitution] The γ-oryzanol derivative is added to the fiber surface layer and / or Alternatively, a modified fiber structure having the inside of a fiber. A method for producing a modified fiber structure, which comprises immersing a fiber structure in a solution of a γ-oryzanol derivative, drying it, and then heat treating the fiber structure at a temperature equal to or higher than the melting point of the oryzanol derivative. A modified fiber structure characterized in that the fiber structure is immersed in a water emulsion prepared by adding an alcohol solution of a γ-oryzanol derivative and treated in a bath at a temperature equal to or higher than the azeotropic point of the water emulsion. Method of manufacturing things. [Effect] The modified fiber structure obtained by the present invention has excellent antibacterial properties and UV cut properties, and also has excellent washing durability. Also, it can be easily applied by post processing, It is highly safe and can be manufactured at low cost. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007314914-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010144315-A |
priorityDate | 1993-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.