http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06256511-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2786295e61d306bf527292c8aea9ff7a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-02 |
filingDate | 1993-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_800118044fc5615e24b57810d14fc37a |
publicationDate | 1994-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06256511-A |
titleOfInvention | Polyaniline derivative and method for producing the same |
abstract | (57) [Abstract] [PROBLEMS] To provide a polyaniline derivative capable of forming a flexible, self-supporting film that is soluble or gellable in an organic solvent, and a method for producing the same. [Structure] The polyaniline derivative has the formula (I): (M, n = 0 or more integers, m / (n + m) = 0 to 1, m + n = Number average molecular weight 2000-5000 consisting of structural units of 10-5000) The polyaniline of 00 has a main chain and has a crosslinked structure of the formula (II), and the number of nitrogen atoms involved in the crosslinked structure is 0.01 to 50% of the nitrogen atoms of the polyaniline of the main chain. [Chemical 2] (In the formula, RP = aliphatic hydrocarbon-based polythiourethane chain having a number average molecular weight of 220 to 100,000, A 1 and A 2 = linking group) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112940218-A |
priorityDate | 1993-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 95.