http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06255009-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 |
filingDate | 1993-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a020414a8bb0b3c407cd6c6f05caf19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_004e81ab95dd0e389031c3aa980ce693 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f2c375127cfa975e63158e75d1f50f9 |
publicationDate | 1994-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06255009-A |
titleOfInvention | Laminated composite |
abstract | (57) [Summary] [Purpose] To provide a laminated composite having excellent adhesiveness between a polyolefin resin foam and a skin material and excellent in moldability. [Composition] Apparent density 0.02-0.2 g / cm 3 , 120 A laminated composite comprising a polyolefin-based resin foam having a xylene extraction residue value of 20 to 80% by weight at 0 ° C. and a skin material, and comprising 60 to 1 of the above polyolefin-based resin foam. Elongation at 20 ° C (JIS K 6767 standard) is 3 The temperature at which the elongation is 50% or more and the maximum elongation is 75 to 1 A laminated composite having a temperature of 15 ° C. and a difference between the temperature at which the expansion of the polyolefin resin foam is maximum and the temperature at which the skin material is maximized is within 15 ° C. [Effect] A molded product without swelling and wrinkles on the surface can be obtained. |
priorityDate | 1993-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 31.