http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0625392-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6cfc033f059d282fcd915bc8be2ae53f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G61-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G61-00 |
filingDate | 1992-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99b0c9628abbf353774cb8979d2cf8f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_536a59ef56e076b3a4835bdab9ff456b |
publicationDate | 1994-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0625392-A |
titleOfInvention | Phenol aralkyl resin and its manufacturing method |
abstract | (57) [Summary] [Structure] Extraction from phenol aralkyl resin obtained by reaction of phenolic compound and aralkyl compound, Phenol aralkyl resin obtained by removing bifunctional components mainly by distillation. [Effect] When the phenolic resin of the present invention is cured with an epoxy resin or hexamethylenetetramine, the viscosity before curing is low and the fluidity is good, so the workability during molding is remarkably improved, and high glass is obtained after curing. It is a resin with a transition temperature and is effective as a base material for friction materials, sealing materials, molding materials, paints and the like. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018100319-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4585255-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006056970-A |
priorityDate | 1992-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 71.