http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06228394-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16J15-00 |
filingDate | 1993-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_421955b177a2330b5fb0d9625bd92fda |
publicationDate | 1994-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06228394-A |
titleOfInvention | Thermoplastic elastomer |
abstract | (57) [Summary] [Objective] To provide a thermoplastic elastomer excellent in the balance between compression set and melt viscosity and excellent in general material strength represented by tensile strength and the like, and a rubber molded article formed by molding the elastomer. To do. [Structure] Polyvinyl chloride resin, core-shell type latex rubber, and plasticizer. 20 to 200 parts by weight of core-shell type latex rubber and plasticizer are added to 100 parts by weight of polyvinyl chloride resin. 1 based on the total weight of polyvinyl chloride resin and core-shell type latex rubber The compression set included in the range of 0 to 200 parts by weight is 40. %, And a tensile strength of 30 kg / cm 2 or more, a thermoplastic elastomer and a molded article thereof. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111902253-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010235834-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018003805-A1 |
priorityDate | 1992-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 50.