http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06207066-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_29180337e1a918cd4b2f6c4e8f664160 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L73-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-08 |
filingDate | 1992-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_48c6ecc4f009dc02433a300c2d1f31d7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6736351e13aaef9205789ec9f8ba0518 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cbacbccc63a8e907852e61fec0ef1994 |
publicationDate | 1994-07-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06207066-A |
titleOfInvention | Thermoplastic resin composition |
abstract | (57) [Summary] [Structure] (A) Styrene resin, (B) polyalkylene oxide glycol, and polyvalent carboxylic acid, polyvalent carboxylic acid lower alkyl ester, polyvalent carboxylic acid anhydride and organic isocyanate. And a high molecular weight compound having an average molecular weight of 10,000 or more prepared by reacting with at least one kind, (C) a modified or unmodified methacrylic resin, and (D) an organic sulfonate, and The thermoplastic resin composition having the compounding ratio of. (1) The mixing amount of the component (B) is 1 ≦ (B) ≦ 30 parts by weight, and the mixing amount of the component (C) is 1 ≦ (per 100 parts by weight of (A) + (B) + (C) in total. C) ≦ 40 parts by weight, (2) the blending weight ratio of component (B) and component (C) is 0.2 ≦ (C) / (B) ≦ 5 (3) The blending weight ratio of the component (B) and the component (D) is 0.01. ≦ (D) / (B) ≦ 0.5 [Effect] A molded article having excellent permanent antistatic property can be obtained. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006273877-A |
priorityDate | 1992-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 97.