http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06172610-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 |
filingDate | 1992-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_04d78fcc8abab11e06161755d388ebba |
publicationDate | 1994-06-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06172610-A |
titleOfInvention | Thermoplastic resin composition |
abstract | (57) [Summary] [Purpose] The molded products after sheet forming and vacuum forming are A resin composition having excellent impact strength, moldability, surface hardness and chemical resistance is obtained. [Constitution] (Component A) In the presence of a diene rubber polymer, Obtained by graft-polymerizing 20 to 90 parts by weight of a monomer mixture consisting of an aromatic vinyl monomer, a vinyl cyanide monomer, and optionally a vinyl monomer copolymerizable therewith, and having a weight average. 20 to 80% by weight of a graft copolymer having a molecular weight in the range of 120,000 to 200,000, (B component) an aromatic vinyl monomer, a vinyl cyanide monomer and a vinyl monomer copolymerizable therewith, if necessary. A copolymer having a relative viscosity η rel in the range of 1.45 ≦ η rel ≦ 1.65 formed by copolymerizing monomers A thermoplastic resin composition comprising 20 to 80% by weight. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5554688-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11208548-B2 |
priorityDate | 1992-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |