abstract |
(57) [Summary] [Structure] (A) Melt flow rate is 50-150g / 10 minutes, 100 parts by weight of a polyphenylene sulfide resin having a small amount of low molecular weight components, (B) 0.1 to 3 parts by weight of a releasing agent such as polyethylene wax, and (C) 20 to 300 of an inorganic filler such as glass fiber. A polyphenylene sulfide resin composition comprising 1 part by weight. [Effect] The resin composition of the present invention is excellent in fluidity and releasability, and exhibits high burr resistance, and is useful for precision molded articles (connectors, etc.). |