Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73e70c68914de121f06dba3fb1f73676 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-189 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 |
filingDate |
1992-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e0f19adb641bbfaf7d799d1d2bab71fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4bd3f5ddff9e9a87de5b105758de6708 |
publicationDate |
1994-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0616835-A |
titleOfInvention |
Polyethylene-2,6-naphthalate film |
abstract |
(57) [Summary] [Object] To provide a polyethylene-2,6-naphthalate film suitable for recycling. [Composition] Melting temperature 300 to 330 ° C., melting time 5 to 3 The intrinsic viscosity after melting under the condition of 0 minutes is 80% of the value before melting. % Or more, and the amount of terminal carboxyl groups after melting is 1 A polyethylene-2,6-naphthalate film having a weight of less than 00 equivalent / 10 6 g. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006016617-A |
priorityDate |
1992-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |