http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06157800-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b0120933550ea729b9f3186c3772531b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 |
filingDate | 1992-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d43869804b6a4ef380ef912d6ccca2b7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0bf73816edc3b70225b97206ad45eb1c |
publicationDate | 1994-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06157800-A |
titleOfInvention | Method for producing polyethylene foam |
abstract | (57) [Abstract] [PROBLEMS] To provide a method for producing a polyethylene foam having excellent tan δ characteristics and transmission loss characteristics. [Structure] Polyethylene foam characterized by using a polyethylene composition in which crosslinked polyethylene fine powder is mixed with polyethylene when a polyethylene foam is manufactured by kneading polyethylene and a foaming agent and heating the resulting kneaded product. It is a body manufacturing method. [Effect] A polyethylene foam having excellent tan δ characteristics and transmission loss characteristics and a good appearance can be manufactured. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005119703-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008500702-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010184969-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4875613-B2 |
priorityDate | 1992-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.