Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_991eae7621f3f352c80792f1d8f19616 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K75-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G101-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F25D23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-14 |
filingDate |
1992-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f76559030d18431b9f70146cbae4cb7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2884d9187a7663de0e34416d892e4dd |
publicationDate |
1994-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H06145406-A |
titleOfInvention |
Heat insulation panel manufacturing method |
abstract |
(57) [Summary] [Purpose] Stop using CCl 3 F. While improving the adhesion between the polyurethane foam and the surface plate, Makes the size of the cells in the polyurethane foam small and uniform to provide excellent heat insulation. [Structure] A method for manufacturing a heat insulating panel by injecting and foaming a foamable urethane raw material liquid into a space S formed by two metal surface plates 1 and a frame 2. 3% by weight or more of CH 3 CCl 2 F is contained in the urethane raw material liquid. The temperature of the surface plate 1 is set to 30 to 50 ° C. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013269340-A1 |
priorityDate |
1992-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |