http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06138703-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 1992-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de18bb67ddbbc590a63f099f11b442ac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c32bd1b62267e9cd3fd595c858d4f02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44b8ccf22f35f2046a77a095165e43cf |
publicationDate | 1994-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06138703-A |
titleOfInvention | Binder resin composition for positively chargeable toner |
abstract | (57) [Summary] [Object] To obtain a binder resin composition suitable for a toner having good fixing property, non-offset property, blocking resistance and moisture resistance and having excellent positive charging property. [Structure] Styrene-acrylic system containing 60 to 95% by weight of a polyester copolymer containing a trihydric or higher polyhydric alcohol and 1 to 40% by weight of an acrylate ester component and / or a methacrylic acid ester component having an ether group. The copolymer has a glass transition temperature of 40 to 68 ° C, a softening temperature of 95 to 165 ° C, and an acid value of 2 A binder resin composition for a positively chargeable toner, which is 0 mgKOH / g or less. |
priorityDate | 1992-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |