http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06130544-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-49845 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 1993-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_156f614e15d29c64fe456f6f33972987 |
publicationDate | 1994-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H06130544-A |
titleOfInvention | Photographic material developable by heat treatment |
abstract | (57) [Summary] (a) At least one binder layer coated on a support (the binder layer comprises at least one photosensitive silver halide and a non-photosensitive silver salt of a fatty acid); and 1) from (b) at least one reducing agent and (c) hexamethylenetetramine and its salts, triazaadamantane and its salts, and hexamethylenetetramine in the binder layer or in another layer in reactive relation with the binder layer. One or more-C The group -S - - H 2, - SO- , or -SO 2 - heat-developable photographic recording material comprising a stabilizer selected from the group consisting of compounds which can be obtained by replacing. [Effect] This material has excellent stability during storage, It is easy and inexpensive to manufacture, and presents minimal environmental or health hazards. |
priorityDate | 1992-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 80.