Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K25-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate |
1992-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75169bdd42220e74b25d121a768d1eeb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26c7e7de6f012a963c67f83bbc60bc7c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d0c3127678b0463942a07a8a395c5dce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23509d8fa73434e9132302edb2727ceb |
publicationDate |
1994-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H06107812-A |
titleOfInvention |
Syndiotactic polystyrene biaxially stretched film |
abstract |
(57) [Summary] [Object] The present invention provides a biaxially stretched syndiotactic polystyrene film, and more specifically, a syndiotactic polystyrene film having excellent heat resistance and good handling properties regardless of the film thickness. The present invention relates to a biaxially stretched film. [Structure] A styrene-based polymer having a substantially syndiotactic structure, the orientation ratio obtained by the following formula is in the range of 0.2-1.5, and the heat shrinkage stress at 200 ° C in the width and longitudinal directions is 200 ° C. Dynamic elastic modulus at 10Hz A biaxially stretched film having a quotient divided by 0.01 or less and a dynamic elastic modulus (10 Hz) at 200 ° C. in the width and longitudinal directions of 1.0 × 10 6 dyne / cm 2 or more. Orientation ratio = Ax / Ay Ax: infrared light polarization direction 1222Cm -1 band intensity Ay when matched with the width direction of the film: the infrared light polarization direction when matched with the longitudinal direction of the film 1222Cm -1 Band strength |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06106616-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0061643-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08323877-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0732468-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H06107813-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6359094-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0724911-A |
priorityDate |
1992-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |