http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0598036-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_88fbcd2a70a3c49d0aed69a000d55909 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L35-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 |
filingDate | 1991-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_585a283adce9e57434b550e8a1193195 |
publicationDate | 1993-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0598036-A |
titleOfInvention | Swelling and softening plastic film |
abstract | (57) [Abstract] [Purpose] To provide a swelling-softening type film suitable for safe PTP packaging that does not damage internal organs even if accidentally swallowed. [Structure] (A) An acrylic resin having a glass transition temperature of 60 ° C. or higher, (B) an acrylic resin having a glass transition temperature of −5 ° C. or lower, and (C) a polyvinyl alcohol resin having an average saponification degree of 60 to 98 mol%. And at least one of the resins (A) and (B) contains a carboxyl group, and the content is 1 to 30% by weight based on the total weight of (A) and (B). It is characterized by Swelling and softening type plastic film. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019073820-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010018678-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011080206-A3 |
priorityDate | 1991-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 63.