Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8aa118fbfa85a6e0cc8c13a8afca19ab |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C21-00 |
filingDate |
1991-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ade2053e0aa6cf3ae79df040e0fdf347 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2be20453bbd808c96ff0561617dad84 |
publicationDate |
1993-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0597479-A |
titleOfInvention |
Method of manufacturing tempered glass |
abstract |
(57) [Summary] [Purpose] By performing ion exchange evenly, It is an object of the present invention to provide a method for manufacturing a tempered glass having high strength at a lower cost than ever before. [Structure] A glass body having an appropriate shape and capable of being chemically strengthened by ion exchange is processed into a desired size, and then the surface thereof is subjected to an erosion treatment with an acid and then subjected to an ion exchange treatment. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2704852-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008306149-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012148955-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101137206-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9426675-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103328396-A |
priorityDate |
1991-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |