http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0585885-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5547f741b25666fc4ae5195cf71a979b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B15-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B29-22 |
filingDate | 1991-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd7bd2e7d371a090a3e1eef913278718 |
publicationDate | 1993-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0585885-A |
titleOfInvention | Method for producing seed crystal for pull-up growth |
abstract | (57) [Abstract] [Purpose] The seed crystal used in the pulling method does not cause cracks in the seed crystal by using a crystal that does not have strain or surface roughness on the surface, Prevents reduction of conduction. [Structure] A seed crystal having a diameter of about 3 mm is grown by the pulling method and used as it is as a seed crystal. Further, the surface of the seed crystal processed into a rod shape having a diameter of 3 mm is laser-annealed to remove processing strain, and the crystal surface is optically smoothed. |
priorityDate | 1991-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6101043 http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451983457 |
Total number of triples: 14.