http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0562159-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5128cfc84a0fb189fceb3cd240c44493 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-23 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-706 |
filingDate | 1991-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef45fa9571f4006fee6eee79b74889b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_723c66cf8358936f4bddff06a7ecf93e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cdf5a76aba88aa6b46eb0d7d38a9945e |
publicationDate | 1993-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0562159-A |
titleOfInvention | Metal fine particle magnetic recording material and manufacturing method thereof |
abstract | (57) [Summary] [Purpose] A magnetic recording material is manufactured by a simpler process than ever before. A recording material capable of both magnetic recording and optical recording is obtained. [Structure] By heating a metal compound in a binder and a reducing agent to react with each other, a composite metal fine particle layer is formed to produce a magnetic recording material. |
priorityDate | 1991-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 63.